Additives and functional resins for coatings and inks
New energy, semiconductor additives
XOANONS® Dispersing agent
Used for preparing SWCNT slurry
Model number
XOANONS®LD 1148-60-2
Specification
Item |
Metric |
Test the method or the equipment |
Criterion of detection |
Composite |
Modified styrene maleic anhydride copolymer solution |
--- |
--- |
Appearance |
Yellow slightly turbid liquid |
--- |
--- |
Content |
50% |
Electric hot blast drying oven |
GB/T 1725-2007 |
Solvent |
1-Methyl-2-pyrrolidone |
--- |
--- |
Density |
1.07-1.12 g/ml |
Specific gravity cup |
GB/T 6750-2007 |
Viscosity |
1000-5000 mPa·s |
Tu-4 viscometer |
GB/T 1723-1993 |
pH value |
9-13 |
Glass electrode method |
GB/T 9724-2007 |
Refractive index |
1.476-1.482 |
Abbe refractometer |
GB/T 6488-2008 |
Note: This data sheet is intended to give typical results, not standard. Subject to COA.
Application system
Solvent-based carbon nanotube slurry and graphene slurry
Property
?Provide steric hindrance, adding it to the slurry can significantly reduce the viscosity of the conductive slurry; Improve the fluidity of the slurry;
?Reduce adverse phenomena such as sedimentation and flocculation of the slurry; The storage stability of the slurry is excellent.
Incorporation
Add the dispersant XOANONS®LD 1148-60-2 to the solvent, stir evenly. Then add it to the slurry according to the formula and grind and disperse it together.
Suggest addition
Addition amount (purchase form) for carbon nanotubes or graphene: 20-100%.
Storage stability
Keep intact 24 months in original package. Products beyond the storage period may continue to be used after inspection. The container must be closed immediately after use.
Package
25KG (plastic drum)