Additives and functional resins for coatings and inks
New energy, semiconductor additives
XOANONS® Dispersant
Dispersion and viscosity reduction of water-based carbon nanotube slurry and graphene
Identification of product
XOANONS®LD1246-60W
Materialization index
Item |
Index |
Test the method or the equipment |
Test standard |
Component |
Modified polyvinylpyrrolidone |
--- |
--- |
Appearance |
Yellow transparent liquid (partially frozen at low temperatures, can be restored by heating, does not affect use) |
--- |
--- |
Content |
50% |
electric drying oven |
GB/T1725-2007 |
Solvent |
Water |
--- |
--- |
Density |
1.09-1.13g/mL |
Specific gravity cup |
GB/T6750-2007 |
Viscosity |
500-2000 mPa.s |
|
GB/T15357-2014 |
pH |
8-13 |
Glass electrode method |
GB/T9724-2007 |
Refractive index |
1.438 -1.442 |
|
GB/T6488-2008 |
Note: This indicator only represents the typical results, and is not regarded as a specification, mainly with specific COA.
Application area
Used for water-based carbon nanotube slurry, graphene slurry
Key property
?Provide steric hindrance, adding it to the slurry can significantly reduce the viscosity of the positive electrode slurry; Improve the fluidity of the slurry;
?Reduce adverse phenomena such as sedimentation and flocculation of the slurry; The storage stability of the slurry is excellent.
Usage method
Add XOANONS®LD 1246-60W to the solvent, stir well and dissolve, then add it to the slurry according to the formula and grind and disperse together. The suitability of the dispersant system can be determined based on the particle size and viscosity of the slurry.
Suggested dosage
Add amount (purchase form) to carbon nanotubes or graphene:20-100%
Storage stability
Seal and store away from light. Unopened in the original package for 24 months. Products beyond the storage period can continue to be used after passing the inspection. The container is not fully used and unprecedented, and must be closed immediately after use.
Pack
25kg(plastic drum)